CC-BY-NC-NDMarilović, DraganaBogdanović, GrozdankaPetrović, Sanja2023-12-262023-12-262023978-86-6305-140-9https://ioc.tfbor.bg.ac.rs/public/2023/Proceedings_IOC_2023.pdfhttps://repozitorijum.tfbor.bg.ac.rs/handle/123456789/2506This paper presents the results of leaching flotation tailings containing 0.13% of copper and 4.22 % of iron. The experiments were carried out in a sulfuric acid solution (H2SO4) and an ionic liquid solution 1-butyl-3-methyl-imidazolium hydrogen sulfate ([bmim]HSO4). Concentrations of the reagents of 0.01 mol/dm3 and 0.05 mol/dm3 were tested. When leaching with sulfuric acid, the leaching degree of copper was 71.05% at the lower concentration of solution and 76.59% at the higher concentration of solution. When flotation tailings was leached in an ionic liquid solution with the same concentrations, the leaching degree of copper was 72.57% (for 0.01 mol/dm3) and 77.10% (for 0.05 mol/dm3), respectively. The results showed that the leaching rate of copper increased in the first 5-10 minutes of the reaction due to the presence of oxide minerals and then slightly increased with time. The dissolution of iron was <3% under the tested conditions. These results indicate that the ionic liquid 1-butyl-3-methyl-imidazolium hydrogen sulfate ([bmim]HSO4) can be used as agent for the leaching process of flotation tailings.enleachingflotation tailingssulfuric acidionic liquidsLeaching of flotation tailings with a solution of sulfuric acid and ionic liquidconferenceObject